The preparation method comprises the following steps that S1, a stainless steel framework is inlaid in the center position of a mold before pouring, fiber paper is wound around the outer side of the framework, and an electrical adhesive tape is wound around the outer side of the fiber paper; s2, a castable with the density not lower than 3.0 g/cm < 3 > is adopted, and integral pouring prefabrication forming is carried out; s3, demolding and taking out the pressed bricks formed by casting, and mounting the pressed bricks above a filter plate; cavities communicated in the vertical direction are formed in the upper end and the lower end of the brick pressing body, longitudinal through grooves are formed in the top and the bottom of the brick pressing body, transverse through grooves perpendicular to the longitudinal through grooves are formed in the bottom of the brick pressing body, and lifting openings are formed in the two sides of the end face, perpendicular to the longitudinal through ...